王建,张海杰,徐秀峰.N2O在CuxFe1-xFe2O4和NixFe1-xFe2O4复合氧化物催化剂上的分解反应[J].分子催化,2015,(1):75-81
N2O在CuxFe1-xFe2O4和NixFe1-xFe2O4复合氧化物催化剂上的分解反应
Catalytic Decomposition of N2O over CuxFe1-xFe2O4 and NixFe1-xFe2O4 Composite Oxides
投稿时间:2014-12-22  修订日期:2015-01-29
DOI:
中文关键词:  N2O催化分解  Cu-Fe复合氧化物  Ni-Fe复合氧化物  催化活性
英文关键词:Catalytic decomposition of N2O  Cu-Fe composite oxides  Ni-Fe composite oxides  catalytic activity
基金项目:山东省科技发展计划项目(2012GSF11708).
作者单位E-mail
王建 烟台大学 s0334139@163.com 
张海杰 烟台大学 xxflab@ytu.edu.cn 
徐秀峰* 烟台大学 化学化工学院 xxf@ytu.edu.cn 
摘要点击次数: 2392
全文下载次数: 3038
中文摘要:
      用共沉淀法制备了一组具有尖晶石结构的Cu-Fe和Ni-Fe复合氧化物,用于有氧条件下催化分解N2O,考察了催化剂组成对催化活性的影响。用N2物理吸附(BET)、X射线衍射(XRD)、H2程序升温还原(H2-TPR)等技术对催化剂进行了结构表征。结果表明:在不同组成的Cu-Fe、Ni-Fe系列复合氧化物催化剂中,CuFe2O4和NiFe2O4对于N2O分解反应的初活性较高,这是因为CuFe2O4和NiFe2O4的比表面积较高、晶粒较小,而且其表面氧物种与金属(Cu2+、Fe3+)的化学作用较弱,氧物种易脱除、脱氧量较高。相比较而言,NiFe2O4催化剂上的N2O分解活化能低于CuFe2O4,NiFe2O4的初活性优于CuFe2O4。500 C连续反应100 h,CuFe2O4上的N2O转化率降至84.9%,而NiFe2O4上的N2O转化率一直保持99%,NiFe2O4有较高的催化稳定性。
英文摘要:
      A series of Cu-Fe and Ni-Fe composite oxides with spinel structure were prepared by a co-precipitation method for N2O decomposition in the presence of oxygen. The effect of composite oxides compositions on catalytic performance was investigated. These catalysts were characterized by means of nitrogen physisorption (BET), X-ray diffraction (XRD) and temperature-programmed reduction of hydrogen (H2-TPR) techniques. It is shown that CuFe2O4 and NiFe2O4 exhibited higher activity for N2O decomposition in Cu-Fe and Ni-Fe composite oxide families, respectively, due to their higher surface area, smaller crystallite, weaker interaction between oxygen species and surface active sites and larger amount of desorbed oxygen in reduction process. The kinetic data suggested that the apparent activation energy (Ea) of N2O decomposition reaction over NiFe2O4 catalyst is lower than that over CuFe2O4 catalyst, thus the catalytic activity of NiFe2O4 is higher than CuFe2O4. After reaction at 500 C for 100 h, the conversion of N2O over CuFe2O4 catalyst declined from 98.7% to 84.9%, whereas N2O conversion over NiFe2O4 always kept 99%. It can be concluded that NiFe2O4 is a stable catalyst in N2O decomposition reaction.
HTML  查看全文  查看/发表评论  下载PDF阅读器